According to different producing technics, there are two kinds of magnetic compounds: injection magnetic compound and extrusion magnetic compound.
Injection magnetic compound is mainly used for producing permanent DC motor, stepper motor, printer and Magrollers of photocopier, bounce cylinder, inductor and Teletron gathering piece. Extrusion magnetic compound is mainly used for producing refrigerator door gaskets and other door seal gaskets.
Typical products of Magnetic Compound
Type |
Magnetic Properties |
Moisture (%) |
|||||
Materials |
Br (mT) |
bHc (kA/m) |
iHc (kA/m) |
(BH)max (kJ/m3 ) |
Testing Method |
||
UMCP-S |
SrFe12O19 |
240±10 |
150±8 |
224±4 |
11.9±0.4 |
injection |
≤0.5 |
UMCP-S1 |
SrFe12O19 |
260±10 |
164±4 |
236±4 |
12.4±0.4 |
injection |
≤0.5 |
UMCP-S2 |
SrFe12O19 |
280±10 |
170±5 |
240±4 |
13.5±0.4 |
injection |
≤0.5 |
UMCP-1 |
BaFe12O19 |
150±10 |
95.5±8 |
183±16 |
4.0±0.4 |
Calendering |
≤0.5 |
UMCP-1b |
BaFe12O19 |
160±5 |
99.5±4 |
199±8 |
4.4±0.4 |
Green piece |
≤0.5 |
UMCP-2 |
BaFe12O19 |
200±10 |
127±8 |
151±8 |
7.2±0.4 |
Calendering |
≤0.5 |
UMCP-2b |
BaFe12O19 |
200±10 |
119±4 |
143±8 |
6.8±0.4 |
Calendering |
≤0.5 |
UMCP-2c |
BaFe12O19 |
200±10 |
119±4 |
143±8 |
6.8±0.4 |
Calendering |
≤0.5 |
UMCP-3 |
SrFe12O19 |
200±10 |
127±8 |
151±16 |
7.1±0.4 |
Calendering |
≤0.5 |
UMCP-3b |
SrFe12O19 |
200±10 |
119±4 |
143±16 |
7.1±0.4 |
Calendering |
≤0.5 |
UMCP-3c |
SrFe12O19 |
200±5 |
119±4 |
143±16 |
7.1±0.4 |
Calendering |
≤0.5 |
Remark
Magnetic properties value measured by calendered flexible magnet.